摘要 |
A method for forming a porous carbonaceous preform includes forming a mixture comprised of up to about 50 volume percent of furfuryl alcohol or tetrahydrofurfuryl alcohol, about 1 to 10 volume percent of a nonionic polyethylene oxide polymer ranging in molecular weight from about 100,000 to 5,000,000, about 30 to 80 volume percent of a carbonaceous material, and the balance water. The mixture is cast to form a body, and heated to decompose the polymer and form the porous preform. A molding composition for carbonaceous material includes, up to about 50 volume percent of furfuryl alcohol or tetrahydrofurfuryl alcohol, about 1 to 10 volume percent of a nonionic polyethylene oxide polymer ranging in molecular weight from about 100,000 to 5,000,000, about 30 to 80 volume percent of the carbonaceous material, and the balance water.
|