发明名称 Silane surface-modified pyrogenic alumina, for use in toner - to increase charge stability, produced by spraying with silane mixt. free from solvent
摘要 <p>Pyrogenic Al2O3 (I) is modified by spraying Al2O3 with 0.5-40 (wt.)% silane mixt. contg. 1-99 pts. trimethoxy-n-octylsilane (MeO)3-Si-(CH2)7-CH3 (II) and 99-1 pts. triethoxy-3-diaminopropylsilane (EtO)3-Si-(CH2)2-CH(NH2)2 (III). The surface-modified Al2O3 (I) has a surface area of 50-150 m2/g, tamped density of 50-90 g/l, drying loss less than 5%, calcination loss of 0.5-15%, C content of 0.5-12% and pH of 4-8. (I) is produced by placing Al2O3 in a mixer and spraying with a mixt. of (II) and (III), then mixing and tempering the mixt. at 100-150 deg.C. USE/ADVANTAGE - (I) is used as additive to toners (claimed) used in copiers and is free from solvent.</p>
申请公布号 DE4202694(C1) 申请公布日期 1993.07.01
申请号 DE19924202694 申请日期 1992.01.31
申请人 DEGUSSA AG, 6000 FRANKFURT, DE 发明人 DEUSSER, HANS, DR., 8757 KARLSTEIN, DE;KERNER, DIETER, DR., 6450 HANAU, DE;MEYER, JUERGEN, DR., 8751 STOCKSTADT, DE;MICHAEL, GUENTHER, DR., 8757 KARLSTEIN, DE;STUEBBE, ANDREAS, 6458 RODENBACH, DE
分类号 C01F7/02;C09C1/40;G03G9/08;G03G9/097 主分类号 C01F7/02
代理机构 代理人
主权项
地址