发明名称 Metal-contg. moulding materials with high thermal conductivity - contain thermotropic polymer, metal filler and phenol], calixarene, polyvinyl-phenol, poly:arylene phosphonate or hydrolysable organo-silane
摘要 Moulding materials (I) are claimed contg. (A) 15-70 wt. % thermotropic polymer, (B) 30-85 wt. % metallic filler and (C) 0.1-10 wt. % cpd. of formula (IIA) (with Mn below 10,000) (IIB), (IIC), (IIC), (IIE) or CH3(CH2)qSiX3 (IIF) R1, R2 = H, 1-22C alkyl or 6-14C aryl; R3 = H, 1-22C alkyl, 6-14C aryl, OH or corresponds to a bracing gp. in residue (A) n = 0-100; R4, R5 = H, 1-22C alkyl or 6-14C aryl (one gp. = H and the other is different from H); R6, R7. 1-22C alkyl or 6-14C aryl (at least one gp. = H); R8 = H, 1-22C alkyl or 6-14C aryl; R9 = H or Me, pref. H; m = 10-500; p = 1-100; X = OMe, OEt, or Cl; q = 0-17. Pref. component (A) has repeating units derived from (a) aromatic hydroxyacids (40-85 mol. %) (b) aromatic amino acids (0-40 mol. %), (c) diphenols (60-15 mol. %) (d) amino-phenols (0-25 mol. %), (e) aromatic dicarboxylic acids and opt. (f) carbonic acid or derivs. thereof. (B) is Al or an alloy of Al with Si, Cu, Mg, Li, and Ti, or Mg or a Mg/Al alloy, pref. Al alone. USE/ADVANTAGE - (I) are moulding materials which can be processed without expensive sintering procedures to give prods. with thermal conductivity higher than that of prior-art materials with the same amt. of metal. The prods. include heat exchangers, casings etc.
申请公布号 DE4141719(A1) 申请公布日期 1993.07.01
申请号 DE19914141719 申请日期 1991.12.18
申请人 BAYER AG, 5090 LEVERKUSEN, DE 发明人 KARBACH, ALEXANDER, DIPL.-CHEM. DR., 4150 KREFELD, DE;ELSNER, THOMAS, DIPL.-CHEM. DR., 4000 DUESSELDORF, DE;KOEHLER, BURKHARDT, DIPL.-CHEM. DR., 4150 KREFELD, DE;OHST, HOLGER, DIPL.-CHEM. DR., 5068 ODENTHAL, DE;WEHRMANN, ROLF, DIPL.-CHEM. DR.;WENDT, ECKHARDT, DIPL.-CHEM. DR., 4150 KREFELD, DE;PIELARTZIK, HARALD, DIPL.-CHEM. DR., PITTSBURGH, US
分类号 C08K3/08;C08K5/13;C08K5/5333;C08K5/54;C08L67/00 主分类号 C08K3/08
代理机构 代理人
主权项
地址