摘要 |
PCT No. PCT/FR90/00375 Sec. 371 Date Jan. 14, 1991 Sec. 102(e) Date Jan. 14, 1991 PCT Filed May 30, 1990 PCT Pub. No. WO90/14909 PCT Pub. Date Dec. 13, 1990.The method for forming a lining on the internal faces (2) of a metallurgical vessel (1) for receiving molten metal involves the following steps: a) at least one movable wall (3) is positioned at a predetermined distance from the internal face (2) of said vessel, b) a composition (4) containing at least one powdered refractory material is introduced between the face (2) of the vessel and the movable wall (3), c) said powdered material is heated so as to agglomerate at least that surface which is intended to come into contact with molten steel, d) said movable wall (3) is displaced and the aforementioned steps are repeated in order to obtain a continuous lining on the internal faces of the vessel. |