摘要 |
A process for spinning para-aramid fibers of increased tenacity and elongation at break by using an air-gap means with a spinneret capillary of less than 2.5 mils diameter, a coagulation bath temperature of less than 10C, and tension on the fibers during washing and drying of more than 0.05 and less than 0.35 gpd.
|