摘要 The present invention relates to a sintered titanium based carbonitride alloy for milling and turning where the hard constituents are based on Ti, Zr, Hf, V, Nb, Ta, Cr, Mo and/or W and 3-25 % binder phase based on Co and/or Ni. The alloy is characterized in that the bottom of crater caused by the crater wear consists of grooves with a mutual distance between their peaks of 40-100 mu m, preferably 50-80 mu m, and where the main part, preferably >75 % of the grooves have a height of >12 mu m, preferably >15 mu m. <IMAGE>