发明名称 Low temperature, high strength, nickel, base brazing alloys
摘要 Brazing of metal parts employing a low temperature, high strength metal alloy is disclosed. The alloy has a composition consisting essentially of about 6.10 to 6.66 atom percent chromium, about 2.43 to 2.46 atom percent iron, about 10.06 to 25.10 atom percent boron, about 3.22 to 12.85 atom percent silicon and the balance essentially nickel and incidental impurities, the composition being such that the total of nickel, chromium and iron ranges from about 71.68 to 74.58 atom percent and the total of boron and silicon ranges from about 25.42 to 28.32 atom percent. Such an alloy is suitable for brazing gamma ' superalloys and stainless steels at temperatures ranging from about 927 DEG -1010 DEG C. to provide strong, low cost joints.
申请公布号 US5158229(A) 申请公布日期 1992.10.27
申请号 US19920826286 申请日期 1992.01.24
申请人 ALLIED-SIGNAL INC. 发明人 BOSE, DEBASIS;DATTA, AMITAVA
分类号 B23K35/30 主分类号 B23K35/30