摘要 |
PURPOSE:To attain high image density, low void and low malodor with low energy. CONSTITUTION:The flash fixation is executed in <=1.8J/cm<2> light energy by using a toner containing a stylene-(meta)acrylic polymer having 30-250 hydroxyl value, a coloring agent and an acrylic ester having >=4C ester part and/or a polymer containing essentially the metacrylic ester having >=4C ester part and having <=8 deg.C glass transition temp. as low Tg additives, a polypropylene wax having 2000-5000mol.wt., aliphatic bisamido wax having 10-30C fatty acid residue group and at least one component selected from antioxidants. |