发明名称 |
Wear-resistant copper-base alloy. |
摘要 |
A wear-resistant copper-base alloy having superior self-lubricity includes, by weight %, Ni: 10.0 to 30.0%; Si: 0.5 to 3%; Co: 2.0 to 15.0%; at least one metal selected from the group consisting of Mo, W, Nb and V: 2.0 to 15.0%; and the balance being Cu and unavoidable impurities, and having a structure in which hard phase grains containing 5 vol% or more of silicide of at least one metal selected from the group consisting of Mo, W, Nb and V are uniformly dispersed in an amount of 10 to 60 vol% in a copper-rich matrix, to which 2.0 to 15.0% of Fe and/or 1.0 to 10.0% of Cr may be further added. <IMAGE> |
申请公布号 |
EP0505172(A1) |
申请公布日期 |
1992.09.23 |
申请号 |
EP19920302348 |
申请日期 |
1992.03.18 |
申请人 |
TOYOTA JIDOSHA KABUSHIKI KAISHA;KABUSHIKI KAISHA TOYOTA CHUO KENKYUSHO |
发明人 |
MORI, KAZUHIKO;KAWASAKI, MINORU;YOSHIDA, SHIN;MURASE, HIROYUKI;SAITO, TAKASHI;TANAKA, KOUJI, NAGAKUTE-RYO 603;SHIMURA, YOSHIO, CRIMSON HEIGHTS 3-C |
分类号 |
C22C1/10;B23K35/30;C22C9/06;C22C29/18;C22C32/00 |
主分类号 |
C22C1/10 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|