摘要 |
Method of constructing deoxidizing bed for gases, containing mixture of copper carbonate with added magnesium and silver carbonate and binding agents and activators formed in discs; is characterised in that the discs are dried in isothermal condition in temperature of 373 K applying continuous neutral gas blow stream with the flow strength 2.5/3 dm<3/cm<2> bed surface h until total humidity removal, temperature is increased to 473 K and the vaporising process is conducted until total removal of the carbon dioxide from the sorbent, the flow intensity of the neutral gas is increased to 8/10 dm<3/cm<2> of bed surface h, with introduction of 15-25% per volume hydrogen maintaining concentration of water steam in gases not exceeding 1.5% per volume, at the conclusion of the steam emission the sorbent is cooled to the environment temperature, using neutral gas mixture stream with 5% hydrogen contents, with intensity maintained.
|