发明名称 |
COMPOSITE MATERIAL CONTAINING SPINEL IN A METAL MATRIX AND PROCESS FOR ITS PREPARATION |
摘要 |
An aluminum matrix composite material is produced containing spinel as the reinforcing material. The spinel which is used has particle sizes in the range of 5-20 mu m and may be of variable composition of MgO:Al2O3 containing 50 to 95 mole % Al2O3 and 50 to 5 mole % MgO. These composites have properties superior to those of the same alloy reinforced with alumina particles. |
申请公布号 |
WO9203585(A1) |
申请公布日期 |
1992.03.05 |
申请号 |
WO1991CA00292 |
申请日期 |
1991.08.19 |
申请人 |
ALCAN INTERNATIONAL LIMITED |
发明人 |
JAIN, MUKESH;NADKARNI, SADASHIV, KASHINATH;MCLEOD, ALAN, DAVID |
分类号 |
C01F7/16;C22C32/00;(IPC1-7):C22C32/00 |
主分类号 |
C01F7/16 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|