摘要 PURPOSE:To obtain a laminate having improved adhesiveness to cloth, improved mechanical strength and dimensional stability, by treating aromatic polyamide fiber cloths by plasma at low temperature, impregnating them with a polyimide adhesive, and subjecting plural sheets of the prepreg to contact bonding under heating. CONSTITUTION:Aromatic polyamide fiber cloths are treated by low-temperature plasma at 0.05-20 Torr gas pressure, impregnated with a polyimide, adhesive, dried, prepared plural sheets of prepreg are piled, and subjected to contact bonding under heating. The low-temperature plasma treatment is carried out by using a mixed gas of oxygen/nitrogen =95/5-5/95 (volume ratio). Preferably the cloths subjected to the low-temperature plasma treatment undergo surface treatment with a coupling agent containing an amino group or epoxy group. The amount of the polyimide adhesive used is 50-250pts.wt. based on 100pts.wt. cloth.
申请公布号 JPH0362179(B2) 申请公布日期 1991.09.25
申请号 JP19850011885 申请日期 1985.01.25
申请人 SHINETSU CHEM IND CO 发明人 UENO SUSUMU;NOMURA HIROKAZU;KURODA KOICHI
分类号 C08J5/06;B29C43/00;B29C43/20;B29K79/00;B29K105/08;B29L9/00;C08J5/24;C08J7/00;D06M10/00;D06M10/02;D06M101/00;D06M101/16;D06M101/30;D06M101/34;D06M101/36 主分类号 C08J5/06
代理机构 代理人
主权项
地址
您可能感兴趣的专利