发明名称 Austenitic steel having superior characteristics in resistance against stress corrosion cracking, method for producing of same and usage of same.
摘要 The present invention relates to an austenitic steel comprising Ni of 9 - 30 %, Cr of 10 - 23 %, and Fe of at least 45 %, which is characterized in comprising enough Cr and Ni to form whole austenitic structure in the equilibrium diagram at 700 DEG C, having austenitic phase at room temperature, and said austenitic phase is a single crystal, and has superior resistance against stress corrosion cracking. The austenitic steel is preferably comprising C </= 0.1 %, Si </= 1 %, Mn </= 2 %, Ni 9 - 15 %, Cr 16 - 18.5 %, and at least one of elements selected from the group of Mo 1 - 3 %, Ti 0.05 - 1 %, and Nb 0.1 - 1.5 %, as of an alloy composition. The alloy relating to the present invention is preferable as a material for members of a reactor core of a nuclear reactor. <IMAGE>
申请公布号 EP0447109(A1) 申请公布日期 1991.09.18
申请号 EP19910301842 申请日期 1991.03.06
申请人 HITACHI, LTD. 发明人 KATO, TAKAHIKO;YOSHINARI, AKIRA;IKEDA, SHINZOO;YAMAMOTO, MICHIYOSHI;KODAMA, HIDYO;SATO, HISASHI;IZUMIYA, MASAKIYO;AONO, YASUHISA
分类号 C22C30/00;C22C38/00;C22C38/40;C22C38/44;C30B11/00;G21C3/07;G21C5/00 主分类号 C22C30/00
代理机构 代理人
主权项
地址
您可能感兴趣的专利