发明名称 |
High temperature silicide protective coating slurry |
摘要 |
A coating slurry comprised of 42 percent silicon and 10 percent chromium metal powders; 45 percent lacquer base including toluene, xylene, and a polymeric binder; and 3 percent antisettling agent. After the slurry has been applied and then subjected to a high temperature vacuum processing, a ceramic coating is obtained which provides 3000 DEG F. high temperature oxidation protection for a refractory tantalum alloy substrate.
|
申请公布号 |
US5043378(A) |
申请公布日期 |
1991.08.27 |
申请号 |
US19910673049 |
申请日期 |
1991.03.21 |
申请人 |
THE UNITED STATES OF AMERICA AS REPRESENTED BY THE SECRETARY OF THE NAVY |
发明人 |
PACKER, CHARLES M.;HENSHALL, CONSTANCE A.;MONTGOMERY, EARL K. |
分类号 |
C09D1/00;C09D133/10;C23C26/02 |
主分类号 |
C09D1/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|