发明名称 METODO PARA PRODUCIR ACERO INOXIDABLE AUSTENITICO ENDURECIDO POR MEDIOS MECANICOS
摘要 A substantially austenitic stainless steel is provided which is characterized by increased strength resulting from martensite formation upon cold working; the stainless steel consists essentially of, in weight percent, 0.08 max. carbon, 0.25 max. nitrogen, 12 to 15 chromium, 6.5 to 8.5 manganese, about 2 to 3.5 nickel, the sum of manganese and nickel being at least 9.0, and balance iron. The steel is further characterized by having less than 15% ferromagnetic phases in the cast and hot-processed conditions. A method of producing the steel product including hot working the steel alloy to a thickness which allows cold working by an amount equivalent to up to 25% thickness reduction and cold working without an intermediate anneal is also provided.
申请公布号 MX162995(B) 申请公布日期 1991.07.30
申请号 MX19840202907 申请日期 1984.10.01
申请人 ALLEGHENY LUDLUM STEEL CORPORATION 发明人 PAUL RICHARD BORNEMAN;JAMES BYRON HILL
分类号 C22C38/00;C21D7/02;C21D7/13;C21D8/00;C21D9/46;C22C38/38;C22C38/58;(IPC1-7):C22C38/40 主分类号 C22C38/00
代理机构 代理人
主权项
地址