In mfg. an uncoated industrial woven material, of high density and low air permeability it is woven from polyamide filament yarns with a hot air shrinkage of 6-15%, measured at 160 deg.C. It is woven in a symmetrical structure, and finished in a watery bath at 60-140 deg.C. The pref. bath temps. are 90-140 deg.C, or 90-100 deg.C.