发明名称 METHOD OF CONDITIONING SURFACES BEFORE PHOSPHATING
摘要 <p>Stabilization of the phosphating quality achieved after a surface conditioning treatment with an otherwise conventional composition containing dispersed colloidal titanium, and other benefits, is achieved by causing the aqueous composition to flow at a rate of at least 80 meters per minute for at least 10 minutes after make-up, in order to achieve optimum titanium particle size and homogeneity of the composition.</p>
申请公布号 WO1991003582(A1) 申请公布日期 1991.03.21
申请号 US1990004998 申请日期 1990.09.04