发明名称 METHOD FOR RECOVERING HIGH PURITY NIOBIUM AND ITS DERIVATIVE FROM NIOBIUM-TITANIUM ALLOY SCRAP OR FERRONIOBIUM
摘要 <p>PURPOSE:To obtain a high purity Nb deriv., etc., by chlorinating Nb alloy scraps, etc., purifying NbCl5 by distillation, reducing the purified NbCl5 with hydrogen, removing Ta, rechlorinating the resulting high purity Nb3Cl8 and allowing the product to react with alcohol. CONSTITUTION:Nb-Ti alloy scraps or ferroniobium is allowed to directly react with Cl2 at >=250 deg.C to continuously obtain anhydrous chlorides and NbCl5 is separated from lower b.p. and higher b.p. chlorides by utilizing the differences in b.p. The purified NbCl5 is reduced with hydrogen, Ta is removed and Mb3Cl8 is recovered and rechlorinated at a low temp. to obtain high purity MbCl5. This NbCl5 is allowed to react with alcohol to obtain high purity Nb alkoxide. This Nb alkoxide is hydrolyzed in the presence of carbon to obtain high purity Nb oxide.</p>
申请公布号 JPH0328333(A) 申请公布日期 1991.02.06
申请号 JP19890162579 申请日期 1989.06.27
申请人 TOSOH CORP 发明人 SUGAWARA HISAO;MACHIZAWA CHUICHI;KAMITARI TOSHIHIKO
分类号 C22B34/24;C01G33/00 主分类号 C22B34/24
代理机构 代理人
主权项
地址