发明名称 METHOD FOR IMPARTING IMPROVED TENSILE-STRENGTH AND IMPROVED FIRE-RESISTANT TO BASIC MATERIAL OF CLOTH
摘要 <p>PURPOSE: To improve tear strength and flame retardancy of a base fabric material by coating an addition type curable silicone elastomer composition including a non-abrasive filler, and coating a composition having contamination resistance. CONSTITUTION: In this method, the addition type curable silicone elastomer composition for coating including 5-300 pts.wt (effective dose) of non-abrasive filler, preferably calcium carbonate, hydrated alumina or the like, per 100 pts.wt of polymer is coated on the base fabric material such as a woven, knitted or nonwoven fabric or the like selected from cotton, polyester, nylon and glass cloth or the like, and coating the composition having contamination resistance, curing and the base fabric material having tear resistance and flame retardancy is obtained.</p>
申请公布号 JPH02300386(A) 申请公布日期 1990.12.12
申请号 JP19890295185 申请日期 1989.11.15
申请人 GENERAL ELECTRIC CO <GE> 发明人 FURANKU JIYOSEFU MODEIKU
分类号 B29B11/16;C09K3/00;C09K3/18;C09K21/14;D03D15/12;D06M11/00;D06M11/44;D06M11/45;D06M11/46;D06M11/48;D06M11/49;D06M11/53;D06M11/55;D06M11/74;D06M11/76;D06M11/79;D06M15/643;D06M15/647;D06M101/00;D06M101/02;D06M101/04;D06M101/06;D06M101/08;D06M101/16;D06M101/30;D06M101/32;D06M101/34;D06M101/36;D06M101/40;D06N3/12;D06N7/00;E04D3/18;E04D5/08 主分类号 B29B11/16
代理机构 代理人
主权项
地址