发明名称 TEIONSHOKETSUKANONASANKABUTSUJISEIZAIRYO
摘要 PCT No. PCT/JP83/00055 Sec. 371 Date Oct. 20, 1983 Sec. 102(e) Date Oct. 23, 1983 PCT Filed Feb. 23, 1983 PCT Pub. No. WO83/03094 PCT Pub. Date Sep. 15, 1983.A low temperature sinterable oxide magnetic material prepared by adding 0.1 to 5% by weight of glass containing 3 to 50 mol % of Li2O, 10 to 97 mol % of B2O3 and 0 to 70 mol % of SiO2 to ferrite containing at least 0.5 mol % of Li2O. Especially, when a glass containing 10-28 mol % of Li2O, 34 to 66 mol % of B2O3, and 15 to 45 mol % of SiO2 is used, the sintering temperature can be reduced to about 1,000 DEG C. or less.
申请公布号 JPH0236534(B2) 申请公布日期 1990.08.17
申请号 JP19820032646 申请日期 1982.03.02
申请人 FUJI ELECTROCHEMICAL CO LTD 发明人 TORII MICHIHIRO;KOSAKA TOMOYOSHI;MAEDA TAKEO;RIKUKAWA HIROSHI
分类号 C01G49/00;C04B35/26;C04B35/64;H01F1/10;H01F1/34;H01F1/37 主分类号 C01G49/00