发明名称 |
Improved halogenated polyester resin and process for the preparation thereof. |
摘要 |
<p>A halogenated polyester composition having improved impact resistance, rigidity and flame retardancy is produced by melt-kneading (A) 99 to 40 weight parts of a halogen-containing aromatic polyester and (B) 1 to 60 weight parts of (B-1) a copolymer of an alpha-olefin and glycidyl ester of an unsaturated acid or (B-2) a graft copolymer of (B-1) and a polymer of units of the formula (1): <CHEM> solidifying the molten mixture by cooling and for at least one hour in an inert gas atmosphere or under a reduced pressure of less than 1.33 kPa (10 torr) and at a temperature greater than 120 DEG C but not greater than the melting point of the mixture, thereby to effect the solid phase reaction.</p> |
申请公布号 |
EP0376613(A2) |
申请公布日期 |
1990.07.04 |
申请号 |
EP19890313394 |
申请日期 |
1989.12.20 |
申请人 |
POLYPLASTICS CO. LTD. |
发明人 |
WADA, MITSUO;USAMI, TAKASHI |
分类号 |
C08F210/00;C08F8/00;C08F255/00;C08F283/02;C08G63/682;C08G63/685;C08G63/78;C08G63/80;C08G81/00;C08G81/02;C08L67/00 |
主分类号 |
C08F210/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|