发明名称 Process of manufacturing seal members having a low friction coefficient
摘要 A process for manufacturing a pair of seal members (10 and 12) such as a pair of disks which control the fluid flow of a faucet. The two seals are formed of a moderately hard material (pb 14), such as stealite, ceramic materials, metal materials or synthetic materials, which can be precisely ground to a particular finish. At least one of the seal members (10) is coated with a thin layer (16) of very hard material such as silicium carbides, metal carbides, metal nitrides, or cubic crystallographic lattice carbons. The coating layer is applied through either physical or chemical vapor deposition. This process provides seal disks with low friction coefficients thereby eliminating the need to provide a lubricant between the cooperating surfaces of the disks. In addition, adhesion between the seals is eliminated despite the smooth surface finish of the disks. Thus, the disks formed through this process improve operation of the faucet or valve utilizing cooperating seal disks.
申请公布号 US4935313(A) 申请公布日期 1990.06.19
申请号 US19880204964 申请日期 1988.06.06
申请人 MASCO CORPORATION OF INDIANA 发明人 KNAPP, ALFONS;BUZZI, GUNTER
分类号 C04B41/50;F16K25/00 主分类号 C04B41/50
代理机构 代理人
主权项
地址
您可能感兴趣的专利