Method of and a spray for manufacturing a titanium alloy |
摘要 |
A method of manufacturing a titanium alloy, wherein a melted and possibly preformed part is annealed to set the starting grain structure, wherewith a first grain structure transformation is accomplished by a first cooling step, whereafter high dislocation densities are produced in the course of a hot forming step, whereupon heat treatment involving a recrystallization is carried out, wherewith in the course of a subsequent cooling a predominantly or substantially martensitic breakdown is achieved, wherewith a grain structure transformation is carried out in a subsequent annealing process, and wherewith in the course of a subsequent chilling a fine grain structure is set. At least the first cooling step is accomplished by spraying the preformed part with water and/or water-air mixtures. A spray device may be used for carrying out the method.
|
申请公布号 |
US4902355(A) |
申请公布日期 |
1990.02.20 |
申请号 |
US19880238050 |
申请日期 |
1988.08.30 |
申请人 |
BOEHLER GMBH |
发明人 |
JAFFEE, ROBERT I.;PUSCHNIK, HERBERT H.;FLADISCHER, JOHANN;MAYERHOFFER, JOHANN;JAGER, HEIMO |
分类号 |
C21D1/667;C22F1/00;C22F1/18 |
主分类号 |
C21D1/667 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|