发明名称 Method of producing a galvannealed steel strip.
摘要 <p>Galvannealed electroplated steel strip. The strip is heated to an alloying temperature of at least about 427 DEG C using an induction coil operated at a frequency to produce an eddy current penetration depth of one-half the strip thickness. The diffusion temperature and time are controlled to minimize the formation of brittle gamma alloy phases in the zinc/iron alloy coating.</p>