摘要 |
<p>Process for the recovery of lithium from a lithium bearing silicate ore in which a concentrate of the lithium bearing silicate ore is mixed with an alkali metal chloride at a mole ratio of 1 to 7 of lithium ion to alkali metal ion. The mixture is heated at a temperature of 900 to 1300°C and the residue is ground with water free ethanol to thereby selectively remove the lithium ion.</p> |