发明名称 Duplex alloy
摘要 A stainless duplex ferritic-austenitic steel with improved corrosion resistance. The steel consists essentially of about: 0.03 w/o Max. carbon, 3.0 w/o Max. manganese, 1.0 w/o Max. silicon, 26.0 to 29.0 w/o chromium, 3.5 to 5.2 w/o nickel, 3.5 w/o Max. molybdenum, 0.15 w/o Min. nitrogen and the balance essentially iron. The steel preferably contains about 0.17 to 0.35 w/o nitrogen for improved pitting resistance and for increased austenite content. Welds of the steel preferably contain at least about 17% austenite in the as-welded condition for improved pitting and intergranular corrosion resistance.
申请公布号 US4832765(A) 申请公布日期 1989.05.23
申请号 US19870015584 申请日期 1987.02.17
申请人 CARPENTER TECHNOLOGY CORPORATION 发明人 DEBOLD, TERRY A.;ENGLEHART, DAVID A.;MARTIN, JAMES W.
分类号 C22C38/00;C22C38/40;C22C38/44 主分类号 C22C38/00