发明名称 |
Anodic coating with enhanced thermal conductivity |
摘要 |
A method of and apparatus for anodization uses an electrolyte consisting of 1.0 percent by weight of aqueous solution of oxalic acid, an anodization temperature in the range of 0 DEG -5 DEG C., and an anodization voltage starting at 100 volts and progressing to 300 volts after 90 minutes at an anodization current density of 2-3 amps per decimeter2 to provide a 30-40 micrometer thickness having a thermal conductivity of 1.3 Watt/meter/C.
|
申请公布号 |
US4822458(A) |
申请公布日期 |
1989.04.18 |
申请号 |
US19880188774 |
申请日期 |
1988.04.25 |
申请人 |
THE UNITED STATES OF AMERICA AS REPRESENTED BY THE SECRETARY OF THE NAVY |
发明人 |
OGDEN, THOMAS R. |
分类号 |
C25D11/10;(IPC1-7):C25D11/10 |
主分类号 |
C25D11/10 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|