摘要 |
PURPOSE:To obtain a thermoplastic resin composition of excellent toughness, impact resistance, heat distortion resistance, moldability and chemical resistance, by using an aromatic polycarbonate, a polyolefin, a modified polyolefin and polybutylene terephthalate. CONSTITUTION:100pts.wt. of (A) 95-5wt.%, preferably 90-10wt.% of an aromatic polycarbonate, preferably a bisphenol A polycarbonate of 10,000-100,000 weight average mol.wt. and (B) 5-95wt.%, preferably 10-90wt.% of a polyolefin, preferably polypropylene are combined with 2-200pts.wt., preferably 5-50pts.wt., respectively, of (C) a polyolefin modified with 0.1-10wt.% of an unsaturated carboxylic acid or its anhydride, preferably free from unreacting monomer, having over 10,000 weight average mol.wt., and (D) polybutylene terephthalate. |