发明名称 PRODUCTION OF MESOPHASE PITCH
摘要 PURPOSE:To obtain the title pitch which can be softened and melted by heating and is suited for use as a raw material for a graphite fiber, by hydrogenating a beta-resin extracted from a coal tar pitch by solvent fractionation and treating the hydrogenation product so as to have a high-boiling point. CONSTITUTION:A coal tar pitch comprising a fraction obtd. by the distillation of a raw tar produced in coal dry distillation is fractionated with a solvent, thereby extracting a beta-resin which is insoluble in toluene, benzene, etc. but soluble in quinoline, pyridine, etc. Then, the resin is hydrogenated and subsequently treated in an inert atmosphere at 360-430 deg.C for 30-300min, so as to have a high-boiling point, thereby obtaining a mesophase pitch having a mesophase content of 80% or higher. Moreover, according to necessity, the pitch is pulverized, and solvent soluble components are removed using benzene or toluene. Thus, there is obtd. a mesophase pitch of 100% in mesophase content which is soluble in 100% quinoline.
申请公布号 JPS6433186(A) 申请公布日期 1989.02.03
申请号 JP19870187749 申请日期 1987.07.29
申请人 NIPPON CARBON CO LTD 发明人 TERANISHI HARUO;YOKOYAMA AKIRA;HARADA HIROBUMI;KAWAI TAKANOBU;HONDA HIDEMASA
分类号 C10C3/04;C01B31/00;C01B31/02;C01B31/04;C10C3/02;C10C3/08;D01F9/14;D01F9/15 主分类号 C10C3/04
代理机构 代理人
主权项
地址