发明名称 LEAD-ACID BATTERY
摘要 PURPOSE:To obtain a lead-acid battery having good initial performance and life performance by using a positive plate containing a vapor phase growth carbon fiber having a specified quantity of acidic functional group. CONSTITUTION:A positive plate containing a vapor phase growth carbon fiber having an acidic functional group of 3-500mueq/g is used. This carbon fiber is prepared in such a way that a carbon source such as hydrocarbon is heated under the existence of catalyst to grow fibrous carbon from vapor phase. The fibrous carbon, crushed or cut fibrous carbon, or heated crushed or cut fibrous carbon is used. At least 0.01 pts. wt. carbon fiber obtained is mixed with 100 pts. wt. lead oxide to produce the positive plate. Thereby, a lead-acid battery having good initial performance and life performance can be obtained.
申请公布号 JPS63248058(A) 申请公布日期 1988.10.14
申请号 JP19870079712 申请日期 1987.04.02
申请人 ASAHI CHEM IND CO LTD 发明人 NAKAMURA KATSUYUKI;KOMATSU YUKINARI
分类号 H01M4/56;H01M4/57;H01M4/62 主分类号 H01M4/56
代理机构 代理人
主权项