摘要 |
ON FORME DES GRANULES CYLINDRIQUES, AYANT UN DIAMETRE DE 8 MM ET UNE LONGUEUR DE 10 A 20 MM, PAR GRANULATION, SOUS UNE PRESSION DE 600 BARS, D'UN MELANGE HOMOGENE DE 952 KG D'ORDURES MENAGERES BROYEES, 50 KG DE CHAUX VIVE ET 5 KG DE CARBONATE DE CALCIUM. ON CHAUFFE LES GRANULES A 200 C, PENDANT 30 MINUTES, DANS UN FOUR TUBULAIRE ROTATIF, DE FACON A OBTENIR 720 KG DE GRANULES AYANT UNE TENEUR EN HUMIDITE D'ENVIRON 1 EN POIDS. ON BROIE FINEMENT CES GRANULES ET ON PREPARE DANS UN MALAXEUR, UN MELANGE FINAL COMPOSE D'UN PREMIER MELANGE DE 101 KG DE CIMENT PORTLAND, 101 KG DE DOLOMIE EN POUDRE, 91 KG DE CARBONATE DE CALCIUM ET 50,5 KG D'EAU AINSI QUE DE LA POUDRE FINE RESULTANT DU BROYAGE DES GRANULES. FINALEMENT, ON GRANULE LE MELANGE FINAL, SOUS UNE PRESSION DE 600 BARS, ET ON LAISSE DURCIR LES GRANULES PAR SUITE DE LA PRISE DU CIMENT. LES GRANULES FINAUX PEUVENT ETRE UTILISES COMME GRANULAT POUR LA PREPARATION DU BETON.
|