摘要 Disclosed herein is a low shrinkable unsaturated polyester resin composition consisting of (A) 20-70% by weight of an unsaturated polyester, (B) 28-60% by weight of a monomer polymerizable with the above unsaturated polyester, and (C) 2-20% by weight of a block copolymer mixture. The mixtures of the monomer (B) and the block copolymer mixture (C), and a mixture of the polyester (A), the monomer (B), and the block copolymer mixture (C) are in a non-aqueous dispersion state. The block copolymer mixture is obtained by polymerizing either one of the monomers defined below in (a) and (b) with a polymerization initiator a polymeric perioxide represented by the formula: <IMAGE> (I) in which R1 represents a divalent branched hydrocarbon group having 10-30 carbons, and R2 and R3 represent a hydrogen atom, a hydroxyl group or an alkali metal, and the average polymerization degree n is 2-40, and is used to obtain a first polymer having peroxy bonds in its molecule, and block-polymerizing the first polymer with the remaining monomer (a) or (b) which has not been used in the first polymerization reaction wherein, (a) is a monomer or a monomer mixture consisting of 70-100% by weight of styrene monomer and 30-0% by weight of a monomer polymerizable therewith. (b) is a monomer or a mixture of monomers consisting of 70-100% by weight of C1-4 alkyl ester of acrylic acid or methacrylic acid and 0-30% by weight of a monomer polymerizable therewith.
申请公布号 JPS6340447(B2) 申请公布日期 1988.08.11
申请号 JP19830248289 申请日期 1983.12.28
申请人 NIPPON OILS & FATS CO LTD 发明人 NAKAYAMA MASAHARU;FUKUSHI KYOSUKE;MORYA YASUO;SUZUKI SHINKICHI
分类号 C08L53/00;C08F283/01;C08F287/00;C08F293/00;C08F295/00;C08F299/04;C08L23/00;C08L51/00;C08L51/02;C08L67/00;C08L67/06;C08L77/00;C08L101/00 主分类号 C08L53/00
代理机构 代理人
主权项
地址