发明名称 BRICK CASTING METHOD FOR STAVE COOLER
摘要 PURPOSE:To mitigate thermal shock on a refractory brick at initial stage of pouring by covering one side face of the refractory brick by a metallic plate and the other side face by a metal wool at the time of casting the refractory brick at working face side of a stave cooler. CONSTITUTION:In the stave cooler, inserting a cooling pipe, which cools furnace wall, etc., of a blast furnace as the cast-in and having the refractory brick 1 at the working face side, few rows, which the plural trapezoid refractory bricks 1 are lined up through asbestos 5, are positioned as parallel at the working face side. Next, the metallic plate 2 having the same quality as the casting 4 on the one side face of the refractory brick 1 contacting with the molten metal of the casting 4 and the metal wool 3 having the same quality as the casting 4 on the other face are abutted, to execute the pouring. Holding heat of the poured molten metal is cooled while conducting to the refractory brick 1 through the metallic plate 2 and the metal wool 3. In this way, the thermal shock to the refractory brick 1 at the initial stage of pouring is mitigated and also the shrinkage force at the time of cooling is absorbed,and the stave cooler having stable construction is obtd.
申请公布号 JPS63192808(A) 申请公布日期 1988.08.10
申请号 JP19870024653 申请日期 1987.02.06
申请人 NIPPON STEEL CORP 发明人 KOGA YASUHIDE;TOMIOKA HIROSHI;MURO YUICHIRO;ICHIKAWA SHINJI
分类号 C21B7/10 主分类号 C21B7/10
代理机构 代理人
主权项
地址