发明名称 |
Eliminating stress relief cracking under welds - by heating adjacent zones |
摘要 |
<p>Formation of fine cracks under welds or weld-coatings can be avoided by locally heating the adjacent zones to a temp. >400 degrees C (pref. about 600 degrees) before or during the welding and immediately thereafter (before cooling).</p> |