发明名称 Process for burning salt-rich coal
摘要 Before salt-rich coal having a chlorine content of at least 5% by weight, a total content of alkali metal chloride and alkali metal sulphate in the ash of the coal of at least 10% by weight, with grain sizes of the coal of less than 12 mm and the ash having a melting point of at most 800@C, is burned, the coal grains are at least partially enveloped with at least one oxide, hydroxide, carbonate or sulphate of calcium or magnesium. The enveloped coal is burned at a maximum temperature which is above the melting point of the ash of the untreated coal. The envelope ensures that the ash does not melt. The coal impregnated by enveloping can be burned in a fluidised bed, in a circulating fluidised bed or else in a kiln with overlying bed. Preferably, the coal pretreated in this way is burned together with inert material.
申请公布号 DE3640908(A1) 申请公布日期 1988.06.01
申请号 DE19863640908 申请日期 1986.11.29
申请人 METALLGESELLSCHAFT AG 发明人 SAMANT,GURUDAS,DIPL.-ING.DR.;HAFKE,CARL,DR.
分类号 C10L9/10;(IPC1-7):F23C11/02 主分类号 C10L9/10
代理机构 代理人
主权项
地址