发明名称 |
Enhanced machining anneal resistant copper alloy |
摘要 |
An enhanced machining oxygen-free copper alloy is provided which contains at least 0.02% by weight silver and from 25 to 100 parts per million sulfur. The copper alloy is anneal resistant and has sufficient ductility to permit cold working.
|
申请公布号 |
US4734254(A) |
申请公布日期 |
1988.03.29 |
申请号 |
US19860941849 |
申请日期 |
1986.12.15 |
申请人 |
THE NIPPERT COMPANY |
发明人 |
NIPPERT, RUSSELL A. |
分类号 |
C22C9/00;(IPC1-7):C22C9/00 |
主分类号 |
C22C9/00 |