<p>PROBLEM TO BE SOLVED: To provide a plastic film laminate for infusion solution showing enhanced oxygen and moisture gas barrier and little elution during storage which is usable for an infusion solution container regulated by the testing method of a plastic-made medicine container according to Japan Pharmacopeia by making a gas barrier plastic film layer thinner. SOLUTION: A gas barrier film laminate is obtained by laminating an inorganic layer 2, a coating layer 3, an adhesive layer 4 and a protective film 5 in this order on at least on one surface of a plastic film 1 wherein the laminate shows a light transmission of not less than 55%, a hue b value of not more than 5, an oxygen transmission of not more than 1 cc/m2.day.atm measured in a dry atmosphere at 40 deg.C and a moisture transmission of not more than 1 cc/m2.day.atm and further the gas barrier plastic film has thickness of not more than 15μm.</p> |