摘要 |
A compn. for thermoplastic resin is presented. Thus, a mixt. contg. 70 parts polybutylene telephthalate, 30 parts poly carbonate, 0.3 part Na-ionomer, and 0.15 part antioxidant in polyethylene vessel is blended. The product shows the following properties; tensile strength = 645 kg/cm2, flexural strength = 902 kg/cm2, flexural elasticity = 2.3X104 kg/cm2, heat modification temp.= 70≦̸C.
|