发明名称 COBALT-NICKEL ALLOY STRIKING SOLUTION
摘要 PURPOSE:To obtain the titled soln. forming uniformly a dense Co-Ni alloy film having satisfactory adhesion by striking by using nickel chloride, cobalt chloride and hydrochloric acid. CONSTITUTION:This Co-Ni alloy striking soln. contains nickel chloride, cobalt chloride and hydrochloric acid or further contains a surfactant as required. When the soln. is used, a dense Co-Ni alloy film having satisfactory adhesion can be uniformly formed by striking as an underlayer on which plating with a noble metal is carried out. A thin noble metallic film having satisfactory heat resistance and adhesion can be formed on the underlayer by plating at a low cost.
申请公布号 JPS62228497(A) 申请公布日期 1987.10.07
申请号 JP19860040297 申请日期 1986.02.27
申请人 NIPPON MINING CO LTD 发明人 ARAKIDA YASUHIRO;FUKAMACHI KAZUHIKO
分类号 C25D3/12;C25D3/56;C25D7/00 主分类号 C25D3/12
代理机构 代理人
主权项
地址