发明名称 CONTINUOUS COKING OF PITCH
摘要 Coke for reactor graphite is produced continuously by coking a hard pitch with a softening point (K.-S.) above 130 DEG C. and a coking residue of at least 45% by weight in a rotary pipe furnace equipped with a moving device and subsequent calcination without intermediate cooling. The temperature of the inner wall of the indirectly heated furnace ranges from about 500 DEG to about 800 DEG C. The gases and vapors formed during the coking process are guided in countercurrent flow to the pitch.
申请公布号 JPS62227991(A) 申请公布日期 1987.10.06
申请号 JP19870060246 申请日期 1987.03.17
申请人 RUETGERSWERKE AG 发明人 MANFUREETO MORUGENSUTERUN;KURAUSU BERUTORANTO
分类号 C10B57/04;C10B55/00 主分类号 C10B57/04
代理机构 代理人
主权项
地址