摘要 |
Elastomeric thermoplastic molding materials contain (A) from 5 to 50 parts by volume of a partially or completely crystalline thermoplastic polymer having a melting point of above 160 DEG C., as a coherent phase, and (B) from 95 to 50 parts by volume of one or more crosslinked elastomeric polymers which are prepared by emulsion polymerization, are dispersed in the component A and have a glass transition temperature Tg of below -10 DEG C., the sum of A and B being 100 parts by volume, with the proviso that the mixture of A and B has a Vicat softening temperature, measured according to DIN 53,460, which is 5 DEG -40 DEG C. lower than that of the component A, with or without (C) effective amounts of conventional assistants.
|