发明名称 IMPROVEMENT OF STRENGTH OF GEAR
摘要 PURPOSE:To considerably improve the fatigue strength of a gear by aging the gear subjected to shot peening after carburization, hardening and tempering so as to convert the surface layer of the gear into a high density hardened layer. CONSTITUTION:A toothed gear is carburized, hardened and tempered. After the surface of the gear is subjected to shot peening, the gear is aged at 100-200 deg.C for 1-2hr. By this method, carbon penetrates into the interstices among the atoms in the surface layer work-hardened by the shot peening, so a high density hardened layer is formed and the fatigue strength of the gear can be considerably improved.
申请公布号 JPS62207822(A) 申请公布日期 1987.09.12
申请号 JP19860050112 申请日期 1986.03.06
申请人 MAZDA MOTOR CORP 发明人 KOJIMA YOSHIHIKO
分类号 C23C8/22;C21D7/06;C21D8/00;C21D9/32 主分类号 C23C8/22