摘要 |
Magnetic thin film storage elements having a biaxial anisotropic characteristic may be grown epitaxially on NaCl, Mg O or other similar crystal materials, and, as described, a film of 80% Ni, 20% Fe is deposited by evaporation in a temperature range of 250-400 DEG C. Use of NaCl is recommended as the films after formation may be floated off in water and picked up on previously prepared strip winding arrays (see Division H3). |