摘要 |
<p>PCT No. PCT/CH84/00101 Sec. 371 Date Feb. 21, 1985 Sec. 102(e) Date Feb. 21, 1985 PCT Filed Jun. 20, 1984 PCT Pub. No. WO85/00127 PCT Pub. Date Jan. 17, 1985.The material according to the present invention comprises a self-flowing alloy containing particularly from 18 to 35% by weight of chromium as well as fractions of boron and silicon in a ratio of 3:4. The alloy also contains from 0.1 to 25.0% by weight of iron, except for the range from 1.5 to 6. The layers obtained by means of said material exhibit a very high resistance to temperatures, particularly also to corrosion and oxidation.</p> |