摘要 |
PURPOSE:To obtain the titled composition of improved weld strength and appearance while retaining deformation resistance, mechanical properties, heat resistance, etc., suitable for structural parts for electrical equipment and automobiles, by incorporating a thermoplastic resin with specified amount of mica with each specific granular size and aspect ratio. CONSTITUTION:The objective composition can be obtained by incorporating (A) a thermoplastic resin (e.g. polyacetal, polyalkylene terephthalate) with (B) 1-60 (pref. 10-50)wt% of mica with an average granular size 0.5-20 (pref. 0.5-10)mum and average aspect ratio >=10 (pref. 10-60).
|