发明名称 METHOD OF LIBERATING NICKEL- AND COBALT-ENRICHED FINES FROM LATERITE ORES
摘要 According to the present invention, Ni- and Co-rich, low Mg fines may be advantageously separated from the coarse fractions of lateritic ores by atmospheric or low pressure leaching. In particular, the process of the present invention comprises contacting a lateritic ore or ore fraction at temperatures from about 20 DEG C. to about 200 DEG C. and pressures from about atmospheric to about 200 psig with an aqueous acid solution to form a leach liquor, a leach residue and a fines fraction. The fines fraction which can be separated from the residue with the leach liquor by conventional means such as cycloning is found to be richer in Ni and Co and lower than the remainder of the residue.
申请公布号 PH20884(A) 申请公布日期 1987.05.27
申请号 PH19500000305 申请日期 1984.04.13
申请人 CALIFORNIA NICKEL CORP. 发明人 LOWENHAUPT HARRIS E.;LITZ JOHN EDWARD;LEEHOWE DENNIS
分类号 C01G51/00;C01G53/00;C01G53/10;C01G55/00;C22B3/00;C22B23/00 主分类号 C01G51/00