摘要 |
<P>LE PROCEDE COMPORTE LA DISSOLUTION SEPAREE, DANS UNE MATIERE VEHICULE EN FUSION 3 D'ELEMENTS D'ADDITION 8, 9, A UNE TEMPERATURE T EGALE A 0,5 A 0,8FOIS LA TEMPERATURE DE LEUR FUSION ET LA SATURATION EN ELEMENTS D'ADDITION 8, 9 DE LA SURFACE DE LA PIECE METALLIQUE 5 A UNE TEMPERATURE T EGALE A 0,3 A 0,5FOIS LA TEMPERATURE DE FUSION DE LA MATIERE DE LADITE PIECE 5, LA DIFFERENCE T-T ETANT EGALE OU SUPERIEURE A 50C. A CETTE FIN, IL EST PREVU DANS LE DISPOSITIF DES CHAMBRES CHAUFFABLES ET COMMUNIQUANT ENTRE ELLES: UNE CHAMBRE CENTRALE 2 RECEVANT DE LA MATIERE VEHICULE EN FUSION 3 ET LA PIECE METALLIQUE 5 A REVETIR ET DEUX CHAMBRES PERIPHERIQUES 6, 7 RECEVANT DE LA MATIERE VEHICULE EN FUSION 3 ET DES ELEMENTS 8, 9 D'ADDITION INDIVIDUELS.</P>
|