发明名称 LUBRICANT FILM THICKNESS MEASURING METHOD OF MAGNETIC DISK MEDIUM
摘要 PURPOSE:To derive easily and exactly a lubricant film thickness in a short time by irradiating X rays of a specified frequency to the surface, and measuring the lubricant film thickness basing on a signal area ratio regarding an intensity of an emitted photoelectron. CONSTITUTION:Both faces of a bustrate 1 are covered with a magnetic material layer 2, and the magnetic material layer 2 is protected by a lubricant holding layer 3 consisting of an inorganic silicon compound whose main component is SiO2, and a lubricant film 4. When this magnetic disk medium is cut to small pieces and irradiated under a high vacuum, a photoelectron jumps out with a constant kinetic energy at every constituent element. A binding energy of oxygen O1s of polyether fluoride being a material quality of the lubricant film 4 is a signal having a peak in the vicinity of 537.1eV, and a peak of a signal of an inorganic silicon compound being a material quality of the lubricant holding layer 3 is in the vicinity of 534.2eV. A lubricant film thickness is measured basing on an area ratio of these two signals.
申请公布号 JPS60128306(A) 申请公布日期 1985.07.09
申请号 JP19830236059 申请日期 1983.12.16
申请人 NIPPON DENSHIN DENWA KOSHA 发明人 HOSHINO MITSUTOSHI;TERADA AKIRA
分类号 G11B5/84;G01B15/02;G01N23/227 主分类号 G11B5/84
代理机构 代理人
主权项
地址