发明名称 Fabrication of high-silica glass article
摘要 Incorporation of fluorine into a porous silica body, such as an unsintered body produced by a sol-gel method, by VAD or OVPO, reduces or eliminates bubble or pore formation upon re-heating of the glass formed by sintering of the porous material. Effective fluorine concentrations are between 0.01 and 5% by weight. The invention can be used advantageously in producing preforms and optical fiber.