<P>PROCEDE DE RECUPERATION DU ZINC A PARTIR DE CENDRES VOLANTES D'UN FOUR METALLURGIQUE.</P><P>ON RECUPERE LE ZINC, ET D'AUTRES METAUX, A PARTIR DES COMPOSES DU TYPE FERRITE DE ZINC FORTEMENT LIES DE LA CENDRE VOLANTE DE FOUR. ON AJOUTE A CETTE CENDRE VOLANTE 1 EN POIDS D'OXYDE DE ZINC LIBRE (SAUF SI L'OXYDE EST DEJA PRESENT). ON TRAITE LA CENDRE VOLANTE DURANT 1HEURE A 750C AVEC UN MELANGE A 20:1 AIR: CHLORE, DE SORTE QUE L'ON ENLEVE DE LA CENDRE VOLANTE, SOUS FORME DE CHLORURES VOLATILISES, LE ZINC, LE PLOMB ET LE CADMIUM.</P><P>APPLICATION: TRAITEMENT DES CENDRES VOLANTES PROVENANT D'UN FOUR A ARC ELECTRIQUE POUR LE RAFFINAGE DE L'ACIER.</P>
|